CCS Grade FQ70 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.180.551.600.0200.0200.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
690770-94014
CCS Grade EQ70 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.200.551.700.0250.0250.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
690770-94014
CCS Grade DQ70 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.210.551.700.0350.0350.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
690770-94014--16
CCS Grade AQ70 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.210.551.700.0300.0300.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
690770-94014
CCS Grade EQ63 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.200.551.700.0250.0250.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
620720-89015
CCS Grade FQ63 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.180.551.600.0200.0200.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
620720-89015
CCS Grade AQ63 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.210.551.700.0300.0300.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
620720-89015
CCS Grade EQ56 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.200.551.700.0250.0250.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
550670-83016
CCS Grade FQ56 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.180.551.600.0200.0200.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
550670-83016
CCS Grade AQ56 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.210.551.600.0300.0300.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
550670-83016
CCS Grade EQ51 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.200.551.700.0250.0250.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
500610-77016
CCS Grade FQ51 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.180.551.600.0200.0200.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
500610-77016
CCS Grade AQ51 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.210.551.700.0300.0300.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
500610-77016
CCS Grade EQ47 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.200.551.700.0250.0250.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
460570-72017
CCS Grade FQ47 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.180.551.600.0200.0200.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
460570-72017
CCS Grade AQ47 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxN max.
0.210.551.700.0300.0300.020

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
460570-72017
CCS Grade EH40 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxAlsNbVTi max.Cu max.Cr max.Ni max.Mo max.N max.
0.180.500.90-1.600.0250.0250.0150.02-0.050.05-0.100.020.350.200.400.08-

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
390510-66020
CCS Grade FH40 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxAlsNbVTi max.Cu max.Cr max.Ni max.Mo max.N max.
0.160.500.90-1.600.0200.0200.0150.02-0.050.05-0.100.020.350.200.800.080.009

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
390510-66020
CCS Grade AH40 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxAlsNbVTi max.Cu max.Cr max.Ni max.Mo max.N max.
0.180.500.90-1.600.0300.0300.0150.02-0.050.05-0.100.020.350.200.400.08-

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
390510-66020
CCS Grade EH36 Shipbuilding Steel Plate
C maxSi maxMnP maxS maxAlsNbVTi max.Cu max.Cr max.Ni max.Mo max.N max.
0.180.500.90-1.600.0250.0250.0150.02-0.050.05-0.100.020.350.200.400.08-

Yield Strength (MPa) min.Tensile Strength (MPa)Elongation min. %
355490-63021